C.2 – CREEP TESTING MACHINES WITH LEVER SPRING MECHANISM

The LABORTECH company offers testing machines for long-term C.2 tests, where a constant load is exerted by a lever mechanism by means of a spring and a control force sensor. All modifications of CREEP test systems C.2 manufactured by us are designed so that the customer can fully rely on its function and accuracy under long-term constant loading (material flow) with force or stress, including elongation and at a constant homogeneous temperature in a high temperature furnace with reliable declaration of results. even after 100,000 hours of continuous loading.

MEZERA

Key features of the C.2 series

Accuracy, coaxiality and durability are the parameters in the standard

MEZERA

  • Material testing machine for classical creep tests with constant gravitational force.
  • Types of tests: crack growth / expansion tests, tear creep tests, rupture tests, classical creep tests.
  • Types of test standards: ISO 204, ASTM E139, EN 2002-005, ASTM E1457.
  • Any load application with controlled force.
  • Vertical stand design with high rigidity, guaranteed mechanical alignment and durability.
  • Constant load using a lever mechanism, weights and gravitational force for more than 100,000 hours.
  • Machine construction in accordance with EN ISO 204, ASTM E 292 and ASTM E139, GOST 10145, GOST 3248.
  • Durable vibrating pads to prevent the transmission of vibrations.
  • Automatic termination of the test after rupture of samples.
  • Automatic leveling of the lever mechanism to the horizontal position.
  • Accuracy class 1 according to ISO 7500-2 -4 to 100% of rated load.
  • LCD SIEMENS integrated into the machine frame, easy to touch, comfort of the machine at a very high level.
  • The machine is controlled by measuring and control electronics SIEMENS S7-1200.
  • Sampling frequency 1000Hz. Resolution level of analog signals ± 32,000 divisions.
  • PC connection – communication via Modbus TCP.
  • Připojení teplotního regulátoru SIEMENS TC-22 přes Modbus RTU.
  • Integrated UPC unit to cover electrical outages.
  • Coaxiality set according to ASTM E1012.
  • Cross cutting edges contribute to axial alignment according to the requirements of ISO 204, ASTM E292, ASTM E139 and NADCAP.
  • Articulated clamping (using cutting edges) in two places.
  • System set by BENTROD unit – evaluation and optimization of concentric and edge alignment correction.
  • Special heating coils for long-term tests with separate thermocouples = field temperature homogeneity.
  • SIEMENS TC-22 temperature controller with precise control built into the machine frame.
  • Wide temperature range with tolerances better than ISO 204 and ASTM E139.
  • One, two or three thermocouples – depending on sample length, material and shape.
  • The integrated intuitive LOTETest test software ensures machine control (gradual release of weights).
  • Data collection and display of measured values from the force channel (if a force sensor is included), the elongation channel and the temperature on the sample as a function of time.
  • CREEPTest software serves as a higher form of data collection, database storage, generation of own methods, etc.
  • Based on their concept and construction, LABORTECH machines comply with all the above-mentioned EC directives on machinery and equipment.
  • Only state-of-the-art safety techniques and proven industrial components working in accordance with the following standards are used: EN ISO 12100: 2011, EN ISO 14120: 2017, EN ISO 60204-1 ed.3, EN ISO 13850: 2017, EN 61000-6-2 ed . 3, EN 614-1 + A1: 2009 etc.

MEZERA

CREEP TESTS C.2 WITH VARIOUS ACCESSORIES

With our range of accessories you will cover all tests…

MEZERA

Testing fixtures

Clamping and centering jigs designed for long-term tests with jigs for high-temperature furnaces. high-temperature high-temperature high-

Materials used: Allooy, Haynes, MAR

Mechanical extensometers

Extensometers for high-temperature furnaces for long-term tests contact up to 1600 °C. high-temperaturehigh-temperaturehigh- temperature

ISO9513 resolution: Class 0.5 ASTME83-10: Class 0.5

Video extensometers

VIDEO extensometers for high-temperature furnaces for long-term tests – non-contact up to 1400 ° C. high-temperature high-temperature high

SO9513 Resolution: Class 0.2 ASTME83-10: Class A

High temperature furnaces

HTF in the temperature range from 200 to 1600 ° C with tolerances better than ISO 204, ASTM E139

Temperature control SIEMENS TC-22 for up to 6 thermocouples.

MEZERA

MEZERA

Do you have questions about our products?

Feel free to contact our product experts.

We look forward to your interest.

–

MEZERA

CHART OF TECHNICAL PARAMETERS series C.2

  • Technical data
  • Product code
  • Maximum load
  • Leverage ratio
  • Machine dimensions
  • Machine height – A
  • Machine width – B
  • Machine depth – C
  • Space height – E*
  • Testspace width – D
  • Machine weight
  • Test speed
  • Max. stroke
  • Measurement accuracy
  • Units
  • –
  • kN
  • –
  • –
  • mm
  • mm
  • mm
  • mm
  • mm
  • kg
  • mm/min
  • mm
  • –
  • 6.10C.2
  • 1.03020319

  • 10
  • 1:20
  • –
  • 2130
  • 1150
  • 700
  • 1460
  • 520
  • 590
  • 50
  • 150
  • ISO 7500-1
  • 6.30C.2
  • 1.03020019

  • 30
  • 1:20
  • –
  • 2280
  • 1150
  • 700
  • 1460
  • 500
  • 665
  • 50
  • 150
  • A class of accuracy 1
  • 6.50C.2
  • 1.03020119

  • 50
  • 1:20
  • –
  • 2280
  • 1150
  • 700
  • 1460
  • 500
  • 665
  • 50
  • 150
  • 0,3 to 100%
  • 6.100C.2
  • 1.03020219
  • 100
  • 1:20
  • –
  • 2280
  • 1150
  • 700
  • 1460
  • 500
  • 665
  • 30
  • 150
  • rated load