C.1 – CREEP TESTING MACHINES WITH LEVER MECHANISM AND WEIGHTS
LABORTECH offers testing machines for long-term tests C.1, where a constant load is derived by a lever mechanism and weight. All modifications of CREEP test systems C.1 manufactured by us are designed so that the customer can fully rely on its function and accuracy under long-term constant loading (material flow) with force or stress, including elongation and at a constant homogeneous temperature in a high temperature furnace with reliable declaration of results. even after 100,000 hours of continuous loading.
Download:
MEZERA
Key features of the C.1 series
Accuracy, concentricity and durability are the parameters in the standard
MEZERA
Types of tests and standards
- Material testing machine for classical creep tests with constant gravitational force.
- Types of tests: crack growth / expansion tests, tear creep tests, rupture tests, classical creep tests.
- Types of test standards: ISO 204, ASTM E139, EN 2002-005, ASTM E1457.
- Any load application with controlled force.
Machine design
- Vertical stand design with high rigidity, guaranteed mechanical alignment and durability.
- Constant load using a lever mechanism, weights and gravitational force for more than 100,000 hours.
- Machine construction in accordance with EN ISO 204, ASTM E 292 and ASTM E139, GOST 10145, GOST 3248.
- Durable vibrating pads to prevent the transmission of vibrations.
- Automatic termination of the test after rupture of samples.
- Automatic leveling of the lever mechanism to the horizontal position.
- Accuracy class 1 according to ISO 7500-2 -4 to 100% of rated load.
Machine operation and machine control
- LCD SIEMENS integrated into the machine frame, easy to touch, comfort of the machine at a very high level.
- The machine is controlled by measuring and control electronics SIEMENS S7-1200.
- Sampling frequency 1000Hz. Resolution level of analog signals ± 32,000 divisions.
- PC connection – communication via Modbus TCP.
- Připojení teplotního regulátoru SIEMENS TC-22 přes Modbus RTU.
- Integrated UPC unit to cover electrical outages.
Axial coaxiality
- Coaxiality set according to ASTM E1012.
- Cross cutting edges contribute to axial alignment according to the requirements of ISO 204, ASTM E292, ASTM E139 and NADCAP.
- Articulated clamping (using cutting edges) in two places.
- System set by BENTROD unit – evaluation and optimization of concentric and edge alignment correction.
High temperature furnace
- Special heating coils for long-term tests with separate thermocouples = field temperature homogeneity.
- SIEMENS TC-22 temperature controller with precise control built into the machine frame.
- Wide temperature range with tolerances better than ISO 204 and ASTM E139.
- One, two or three thermocouples – depending on sample length, material and shape.
Control software
- The integrated intuitive LOTETest test software ensures machine control (gradual release of weights).
- Data collection and display of measured values from the force channel (if a force sensor is included), the elongation channel and the temperature on the sample as a function of time.
- CREEPTest software serves as a higher form of data collection, database storage, generation of own methods, etc.
Safety
- Based on their concept and construction, LABORTECH machines comply with all the above-mentioned EC directives on machinery and equipment.
- Only state-of-the-art safety techniques and proven industrial components working in accordance with the following standards are used: EN ISO 12100: 2011, EN ISO 14120: 2017, EN ISO 60204-1 ed.3, EN ISO 13850: 2017, EN 61000-6-2 ed . 3, EN 614-1 + A1: 2009 etc.
MEZERA
CREEPTest C.1 TESTS WITH VARIOUS ACCESSORIES
With our range of accessories you will cover all tests…
MEZERA
Testing fixtures
Clamping and centering jigs designed for long-term tests with jigs for high-temperature furnaces. high-temperaturehigh-temperature high-temperaturehigh-
Materials used: Allooy, Haynes, MAR
Mechanical extensometers
Extensometers for high-temperature furnaces for long-term tests – contact up to 1600 ° C. high-temperaturehigh-temper high-temperaturehigh-temper
ISO9513 resolution: Class 0.5 ASTME83-10: Class 0.5
Video extensometers
VIDEO extensometers for high-temperature furnaces for long-term tests – non-contact up to 1400 ° C. high-temperaturehigh- high-temperaturehigh-te
SO9513 Resolution: Class 0.2 ASTME83-10: Class A
High temperature furnaces
High temperature furnaces in the temperature range from 200 to 1600 °C with tolerances better than ISO 204, ASTM E139.
Temperature control SIEMENS TC-22 for up to 6 thermocouples.
MEZERA
Do you have questions about our products?
Feel free to contact our product experts.
We look forward to your interest.
–
MEZERA
TABLE OF TECHNICAL PARAMETERS series C.1
- Technical data
- Product code
- Maximal Load
- Lever ratio
- Machine dimensions
- Machine height – A
- Machine width – B
- Machine depth – C
- Space height – E*
- Space width – D
- Machine weight
- Test speed
- Max. stroke
- Measurement accuracy
- Units
- –
- kN
- –
- –
- mm
- mm
- mm
- mm
- mm
- kg
- mm/min
- mm
- –
- 6.10C.1
- 1.03010420
- 10
- 1:20
- –
- 2130
- 1150
- 700
- 1460
- 520
- 590
- 50
- 150
- ISO 7500-2
- 6.30C.1
- 1.03010019
- 30
- 1:20
- –
- 2280
- 1150
- 700
- 1460
- 500
- 665
- 50
- 150
- Class of accuracy 1
- 6.50C.1
- 1.03010119
- 50
- 1:20
- –
- 2280
- 1150
- 700
- 1460
- 500
- 665
- 50
- 150
- 4 to 100%
- 6.100C.1
- 1.03010219
- 100
- 1:20
- –
- 2280
- 1150
- 700
- 1460
- 500
- 665
- 30
- 150
- rated load